| Volatilizes water and selenium by heating the de-coppered slime produced after copper electrolysis between 450 and 650¡É. | |
|
 |
| Recovers crude Selenium (99.9% Se) from the Selenious acid (H2SeO3) solution using SO2 Gas in the Circulation tank. | |
|
 |
| Produces selenium products with a purity of 99.95% by melting the crude selenium from circulation tank at 320¡É | |
|
 |
| Casts of silver anode after melting and refining the roasted slime is mixed with Flux in the TROF. | |
|
 |
| Produces silver products by melting and casting silver crystals with a purity of 99.99% produced by electrolyzing the Ag Anode, which is produced during TROF. | |
|
 |
| Extracts crude gold by dissolving the Ag slimes by nitric acid. | |
|
 |
| Casts the gold Anode by melting crude gold produced in the leaching process. | |
|
 |
| Produces gold products by melting and casting the Cathode with a purity of 99.99% by electrolyzing gold anode. | |
|
 |
| Extracts PdO-Slime from Pd in the solution after eliminating gold from gold sand in Ag slimes in the leaching process. | |
|
 |
| Produces Palladium products with a purity of 99.9% by oxidizing and reducing the extracted PdO-Slime in the concentration reaction. | |
|
 |
| Produces platinum products with a purity of 99.8% by oxidizing and reducing Pt-Slime and extracting Pt from the gold electrolyte for gold electro-refining. | |